[MW:29879] Welder qualification as per Chapter IX of ASME B31.3.

Dear Experts,

As per ASME B31.3  Chapter IX Welding, does performance qualification requires all mechanical testing to do be done including tensile, bend, impact, lateral expansion to be measured apart form RT.

As per Clause K328.2.1(e)

(e) Mechanical testing is required for all performance
qualification tests.

Pl share your valuable inputs.

best regards

Kataiah



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFM%2B2hzyD_p1qtymWBGz%2BcnBdN%3Djqj7ms0tejXDKvG0uQU2ryA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...