Position  is essential  variable you have to in 3G also, 

On Thu, 20 Jun 2019, 17:52 K K, <karan.hbl@gmail.com> wrote:
Dear Experts,

Please clarify me regarding below mentioned doubts.
As per AWS D1.1

1)      As per PQR thickness qualified with 25mm(Test coupon )


But In WPS thickness mentioned 28MM ( 3.2mm to unlimited )

 

As per AWS D1.1 Table   4.2

For thickness range is qualified for 25 mm ( 3mm to 2T) if i am correct.


2)   Regarding Position – PQR is qualified with 2G( Horizontal)

But in WPS welding Progression – Uphill. whether 2G can weld Uphill position. 


Please clarify me regarding above points.


Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eed99218-5c5c-42df-a5f2-dd072a39d346%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD2W9vyAV-jAdqQAFmucuyCyjHbANYdb3urgFHd5FD4jdZG_bQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...