As such no difference as far as MTC concerned.  ASME starts  with SA and ASTM with A . For example ASTM-A-106  and ASME-SA-106 . But ASME dose not cover all items of ASTM.   American National Standards Institute, also abbreviated as ANSI, and the American Society of Mechanical Engineers, also abbreviated as ASME, are both non-profit organizations mainly focusing on bringing uniformity in voluntary standards used in the engineering discipline. code – also known as ASME Boiler & Pressure Vessel Code or BPVC – is the standard that regulates the design, development and construction of boilers and pressure vessels utilized in a variety of industries. ASME takes reference of ASTM in it's publications, so when you raising requisition for any product, such as Valve whose dimensions are defined in ASME B 16.34, you need to refer respective ASTM standards, like A105 if the valve is to made out of forging.

On Fri, 14 Jun 2019 at 21:28, Pankaj Kolhe <pankaj.kolhe15@gmail.com> wrote:
Dear experts,

what is the difference in ASTM and ASME material. what care should be taken while reviewing MTC, and lab testing.
when can we say this material is acceptable as per ASTM OR ASME?

Pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_HBVuSzAyetS1DzmjbzbP8%2BDN6L3PPx2ZCjDfuni9rbyJW6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjbjB%2BdTj4r4gpaZKK86xW%2B32xrKMiZqF1qv-miwU10sg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...