Re: [MW:29724] Suitable TIG Welding Filler wire & Electrode for welding ASTM-B. Gr. 2.: ( ASTM B265 Grade 2 ) material with SS316L grade material.

Fusion welding not possible. Try with silver brazing. Thanks

On Tue, 18 Jun 2019 3:29 pm Gopi Krishna Banerjee, <gopikrishna.banerjee@gmail.com> wrote:

Pleas help me to Select Suitable TIG Welding  Filler wire & Stick Welding Electrode and welding procedure for welding ASTM-B. Gr. 2.  ( ASTM B265 Grade 2 ) material with SS-316L grade material.  316L, Grade plate thickness is 20mm & Titanium plate thickness is 8 mm.

Using ASME IX Code.  
Thanks &  Best Regards.

G. K. Banerjee.

Welder Trainer.

Nagpur.M.S. India.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGhQL0miUo9_FuLS1d-BiToY6gNT8LR8mOFmzBwSUuSybh4zkg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePp3wwFmfpvxZR8d0FgvhzhKPH4zHE68%3DUd8GdwqLi6gA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...