Re: [MW:29724] Difference in ASTM and ASME material

Not all ASTM materials are qualified as per ASME standards.
Each ASME standard accepts ASTM materials based on the application.
 
Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Fri, Jun 14, 2019 at 8:28 PM Pankaj Kolhe <pankaj.kolhe15@gmail.com> wrote:
Dear experts,

what is the difference in ASTM and ASME material. what care should be taken while reviewing MTC, and lab testing.
when can we say this material is acceptable as per ASTM OR ASME?

Pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_HBVuSzAyetS1DzmjbzbP8%2BDN6L3PPx2ZCjDfuni9rbyJW6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiHYzBAKFOV2ZDaPrXn97SBaRiLEzzu8qYFaJ-WbCsB4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...