Re: [MW:29715] Difference in ASTM and ASME material

There is a difference at first glance, the ASTM materials start with A, for example A36, when they are ASME, the name starts with SA, for example SA-36, the S indicates that that material specification was adopted by ASME, but if you compare a material A36 Vs SA-36, the chemical composition and physical properties are the same, another big difference that we can see is that not all ASTM materials are ASME materials, that is, the ASTM list of materials is much larger than the list of ASME materials (Table QW-422), since the list of ASME materials, are materials whose purpose is the manufacture of boilers and pressure vessels.
Regards!.

El vie., 14 jun. 2019 a las 10:58, Pankaj Kolhe (<pankaj.kolhe15@gmail.com>) escribió:
Dear experts,

what is the difference in ASTM and ASME material. what care should be taken while reviewing MTC, and lab testing.
when can we say this material is acceptable as per ASTM OR ASME?

Pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_HBVuSzAyetS1DzmjbzbP8%2BDN6L3PPx2ZCjDfuni9rbyJW6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLygQ9StJ4hpUfNoqdJW83eM5-sh80bRjHagV9KiNjUew%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...