     Dear Sir,


    Actually I need to Qualify the WPS for 6GR position as per AWS D1.1.  

As per Clause no 9.15.4.1, it is clear that Mock up test coupons need to be welded.My concern is about the size ofspecimen to be used for Sample Mock up test. Whether we can use Plates (Since it is mentioned Sample joint) instead of tubular sections. Also whether  points a,b,c applicable for only plates.??


Thanking You,

Sandeep.P.R 



















 
On Fri, Jul 2, 2010 at 8:59 PM, Philip, Taiye (Lagos) <Taiye...@deltaafrik.com> wrote:

Hello gents,

 

 I have a query on butt joint welding with 6GR qualified welder. As per AWS D1.1 (2006) Table 4.10 Note d, 6GR qualified welder is qualified for all position. However, they are not qualified to weld production weld butt joint welded from one side without backing or welded from both side without backing. In this case, it is considered as single side welding without backing. Pls could some one in the house clarify more on these if I am right or wrong as per D1.1 interpretations?

 

 

Regards

Philip Taiye

Principal QA/QC Welding Engineer

(MIPs Quality Control)

DeltaAfrik Engineering Limited

2nd Floor, City Express Bank Building

Plot 1637 Adetokunbo Ademola Street

Victoria Island, Lagos  Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418

e-mail: taiye...@worleyparsons.com

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d4a1ce4-2c08-45f1-9347-b045e46bb842%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...