Re: [MW:29696] Welding EN19 to IS 2062

Extra photos without DP

On Thu, Jun 6, 2019, 9:15 PM Mohamed Elsahhar <mohamed.elsahhar2000@gmail.com> wrote:
Dear Gents,
Could you plss share extra photos 

On Thu, Jun 6, 2019, 1:40 PM Somnath Ashtakar <s.ashtakar@gmail.com> wrote:
Hi experts,

I am doing welding of EN19 round bar 
( dia 80mm ) to IS 2062 E250 BR (25mm thk) plate using E71T-1 electrode
( preheat 150deg & then slow cooling),but getting discontinuities after welding which seems like crack.

Can someone please suggest me right electrode and procedure..

Thanks in advance.

Attached photos for reference.


Regards,
Somnath
9096297210

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EaZvkhbPN7V4dQJKVaSAn2McKuwRZ5enA8KOvVJOV%3Dn9w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADGm7%3Dy6HFAG824-Zxvc82Y%3DAn2vnsGhFRzrx-gJY16J-nVP-A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EYyWR_fJRuLkq_Y-K5-cK7mRJAasx50Q2XK8M4VDy13ow%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...