Re: [MW:29681] failure in PV due to MIC corrosion

INTERESTING, THANKS

Στις Σάβ, 25 Μαΐ 2019 στις 8:44 π.μ., ο/η Tadic, Miroslav <Miroslav.Tadic@ypfbchaco.com.bo> έγραψε:
        Dear Group

Just to share with you this indication.

It´s about a failure in the bottom zone of pressure vessel separator.

This is a thickness lost due to corrosion by bacteria or MIC as is mentioned in API 571

This indication has more than 2 meter in longitude and 0.6 meter in wide.

Nominal wall thickness 3/8".

Failure presented after 15 years in service of pressure vessel.

Regards

Miroslav Tadic
Integrity Engineer
API 581 IPC  # 60883



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C80362EFAB0D%40BOLEXVSG11.chaco.com.bo.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AJY0LyBJWTVNct9dqK8njdKbp6zVs0Omj2G%2B4JWN0omQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...