Re: [MW:29678] Charpy vee notch toughness

Hi,
Is this a general query ?
For general query you have to go the applicable code like ASME b 31.3 for piping and 31.4 or 31.8 for pipeline.

If you have any specific query for the particular material and MDMT than it can be answered.

On Jun 2, 2019 9:42 PM, "Khaled lamraoui" <EURL.LHG@gmail.com> wrote:
Dear expert.                                  Please I need your help about the requirements of charpy vee notch toughness for piping and pipeline I mean when the test will be required.           I appreciate your help

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4adaf67b-388d-430d-bd1b-95ec89b8dc8f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCTPZ%3DnVKeccbjmEVGY_5u59Tj28h8rUJ67YofH2Uygcg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...