[MW:29762] Usage of SS304 tubes ot SS316L tubes in cooling water exchangers

Recently I observed that in one of the cooling water exchanger (tube in tube) which has Hydrogen at 230DegC on the outer tube and cooling water on the inner tube. The tube metallurgy was SS304. 
Where as in another unit, a cooling water exchanger with SS 316L tubes had lean amine on shell side. 

On what basis is 316L tubes chosen over 304  tubes when a cooling water exchanger is designed?

 - I have two things in mind as far as corrosion is concerned, one being ClSCC and another being PTASCC. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/12819d80-1e2a-471d-bf6b-835e257ed115%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...