Dears ,

Could you please let me know whether PWHT is required for piping as per ASME B31.3, 2016 Edition for the P No. 1 Gr.1 welded to itself and also welded with  P No. 1 Gr.2 up to 25 mm thickness of welds, as per the Table 331.1.1.

Also, there is an exemption given in Table 331.1.3, when we preheat of 95 Deg C for greater than 25 mm thk. Hence I am asking this query.

Please check and let me know.

With best regards,
Saravanan Sornam,
Korea

.




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2BDAp2af%3D95av%3Do3qqX-6mz63SL0vT84D4cOcF%2BrjM0PA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...