Dear Experts,

I have some difficulty to interpret the requirements of ASME section IX

I have a  PQR Based on a dual process GTAW+SMAW ( 8 mm+9.48 mm) on an 17.48 mm ( 24" NPS ) butt weld.

If i am use this PQR what would be my thickness range in WPS  a) Weld metal thickness range for GTAW + SMAW ? b) And what is the base metal thickness range ?

If i set in WPS base metal thickness 13.1 mm to 26.2 mm is it ok / If no than please let me know way i can't set this range.

And weld metal thickness range for GTAW - 14 mm and SMAW - 18.5 mm .

Please give with details explanation regarding my above difficulty.

Thanks and Regards
Kiran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/85413d61-938b-4d05-b22c-1c598eb6ac5d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...