[MW:29719] Re: AISI 4130 and API 5CT Well Head Casing

A5.5 E11018-M, easy to order.
Cooling rate control is important and PWHT to reduce stress.


On Wednesday, June 12, 2019 at 12:22:55 PM UTC+7, Ehab Ahmed wrote:
Dear Sirs, 

Pleas help me to Select electrode ? for AISI 4130 (70-75 Ksi) and API 5CT L80 Pipe materials to weld by SMAW. 

Using ASME IX Code.  

Thanks and Best Regards,
Ehab Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8da69c59-1000-4b6b-a8b6-e7a86496fab8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...