[MW:29719] Aluminium bronze to CuNi 90/10 base metal welding

Dear Experts,
Greetings!
Which welding consumables Is good for aluminium bronze to CuNi 90/10 base metal Welding? Recently we used CuNi 90/10 but we observed crack in weld metal, your positive reply is so valuable to us.

With Regards


Rahul J Rathod 
Welding Technician 

What's up +9181155889118?

 view my profile onLinkedIn view my profile on facebook my skype id

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANaNbfm9NPR%2BceeQvvsFt2-rtyRbedQnQ3d8b6NOiWsQobK2Cg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...