Monday, October 8, 2018

Re: Re: [MW:28404] Tack welder qualification

Could u pl give ASME code ref for Tack welder qualification. 
General Engineering Practice is entirely different.
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Oct 8, 2018 at 9:23 AM Prakash Gotimukul <gprakash31@gmail.com> wrote:
Any welder welding on pressure part must be a qualified welder incl tacks. There is no concession given in code for tack welders. All are qualufied welders. Some may be less experienced. Those u can use for tacks. But qualified Yes. Unqualufied welders shd not even touch pr parts.

Rgds Prakash Gotimukul AIS

On Mon, 8 Oct 2018, 07:43 muneebslsa@gmail.com, <muneebslsa@gmail.com> wrote:
Greetings,

It is not the tack welder qualification for tack, or not even a fillet qualification for a tack in groove, but it is the qualification of welder and welding operators in groove welds who qualifies the tack as per trailing mail it is very clear that ASME B 31.3 interpretations are stirngent saying fillet qualified groove tacks also? its says no...

So in your case same applies you dont need a tack qualified welder to tack a weld, but a qualified grooved welder.

If i am in your place, i will choose the poor performance welder though are qualified, but still not consistent to get a qualified weld or a repair welder or a welder who is in revoking stages, if you quantify you will get a  sum to accompay in your tack bay, this everything comes under planning and not leaving loop holes for TPIs, if you are following as per written documents.

or

If your client or TPIs are bold or wise thinkers to know the consequences of flushed off tacks then it is not a big deal but take a verbal approval for non qualified welder, but you make sure they are good enough to make tacks.

Hope its clear.

SAES-W-011
8 Welder and Welding Operator Qualification
8.1 All welders, welding operators, brazers, and brazing operators shall be qualified in accordance with the ASME SEC IX and SAEP-321, SAEP-322, SAEP-323, and SAEP-324,
as applicable, for all welding, including tack, temporary, and repair welds.

Regards,
Mohamed Muneeb Mahaboob.


 
Date: 2018-10-08 06:45
Subject: Re: [MW:28401] Tack welder qualification
Ok noted but my tack welders are working at fitup section and welders are working at Welding area.my concern is that how I am sure that my tack welder is qualified tack welder.is there any test is required?

On Mon, 8 Oct 2018 at 7:41 AM, Mohamed Muneeb <muneebslsa@gmail.com> wrote:
Also if SA company project then required. 

On Sun, Oct 7, 2018, 5:02 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
What is the code of contruction. If it is AWS D1.1, yes required. But otherwise no. 

On Sun, 7 Oct 2018 3:34 pm SUNILKAUSHIK, <sunilkaushik08@gmail.com> wrote:
Dear sir,
           I am working in fabrication company of piping.My company divided the the welders in two different area-(1) tack welders & (2) welders.Tack welders are working at fitup section & welders are working in welding area.Now my question is that-is it required to qualify the tack welders?If yes then why? If yes than how i will proceed & how to make the prolongation of tack welders?

On Thursday, 15 December 2011 20:22:28 UTC+5:30, samshuddin k wrote:
Dear Sir
Thanks for your guidance.
Still I am not clear with the concept
ASME Sec IX says all welding shall be done by a qualified welder, So
for tacking groove joint,
welder need to be qualified for groove joint.....?
Or if he qualified for fillet joint, he can allowed for tacking groove
joint (Tack either incorporated into the final weld or removed).....?
please reply
Samshuddin.K
Asst Engineer-QSA
N-KOM

On 12/13/11, Morin, Darcy (Bantrel Management Services)
<Mor...@bantrelmanagementservices.com> wrote:
> ASME IX recognizes "Welders and Welding Operators".  There is no provision
> for "Tack Welders" in ASME IX.  However, ASME B31.3 328.5.1(c) mentions
> "Tack Welders", and here is the subsequent Interpretation of this clause:
>
>
>
> Interpretation 22-35
>
> Subject: ASME B31.3-2008, Para. 328.5.1(c), Tack Welding Welder Performance
> Qualifications
> Date Issued: October 5, 2009
> File: 09-1003
> Question (1): Does ASME B31.3, para. 328.5.1(c) require that tack welds,
> whether they are to
> be incorporated into the final weld or be removed, be made by a qualified
> welder?
> Reply (1): Yes.
> Question (2): Does ASME B31.3, para. 328.5.1(c) require that tack welds be
> made to a qualified
> WPS for that joint?
> Reply (2): Yes; see para. 328.5.1(a).
> Question (3): Does ASME B31.3, para. 328.5.1(c) allow tack welds on a groove
> weld joint to be
> made by a welder qualified on a fillet weld test?
> Reply (3): No. See ASME BPV Code Section IX, para. 303.2.
>
>
> Regards,
>
> Darcy Morin
>
> Bantrel Management Services
> mor...@bantrel.com
> o - 780 979 6225
> c - 780 782 5692
>
> -----Original Message-----
> From: material...@googlegroups.com
> [mailto:material...@googlegroups.com] On Behalf Of samshuddin k
> Sent: December 13, 2011 9:49 AM
> To: materials-welding
> Subject: [MW:13203] Tack welder qualification
>
> Dear Experts
> There is any clause in ASME Sec. IX for tack welder qualification.
> Which Code explains tack welder qualification for piping regards
> Samshuddin.K
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> This e-mail and any attachments may contain confidential and
> privileged information. If you are not the intended recipient,
> please notify the sender immediately by return e-mail, delete
> this e-mail and destroy any copies.
>
> Any dissemination or use of this information by a person other
> than the intended recipient is unauthorized and may be illegal.
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone