Hi Hasin,

 

Please refer  the extracts of the following clauses of API-650, related to welding procedure and welders qualification. ASME Sec-IX is should be  good for both.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

9.2 Qualification of Welding Procedures

9.2.1 General Requirements

9.2.1.1

·         The erection Manufacturer and the fabrication Manufacturer if other than the erection Manufacturer, shall prepare welding procedure specifications and shall perform tests as required by Section IX of the ASME Code.

·         Welding procedures for ladder and platform assemblies, handrails, stairways, and other miscellaneous assemblies, but not their attachments to the tank, shall comply with either AWS D1.1, AWS D1.6, or Section IX of the ASME Code, including the use of standard WPSs.

 

9.3 Qualification of Welders

9.3.1

.

9.3.2 The welders and welding operators who weld pressure parts and join non-pressure parts, such as all permanent and temporary clips and lugs, to pressure parts shall be qualified in accordance with Section IX of the

ASME Code.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hasin Shaikh
Sent: December 7, 2017 4:19 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27136] IAWS D 1.1 ALLOWS ASME SEC IX WPS/WQT?

 

It is in terminal project where tank design code API 650 & Related piping as per ASME B31.3

 

where have structural work as well

 

On Thu, Dec 7, 2017 at 12:18 PM, Dinesh Somwanshi <som.din@gmail.com> wrote:

Is it scope of work for structural welding, ASME 9 For piping scope.

 

Additionally need to verify about your project specifications details.


Thanks & Regards

 

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

 

On Thu, Dec 7, 2017 at 3:21 PM, Hasin Shaikh <hasin.shaikh@gmail.com> wrote:


Hello To everyone

 

My question about AWS D 1.1 & ASME SEC IX

 

IF i have wps/pqr and welder qualification according to ASME SEC IX can i use the same with structural fabrication and welding with reference of code of AWS D 1.1?

 

or i need to establishe separate WPS/PQR and welder qualification according to AWS D 1.1? 

--

*With Regards
Shaikh.Hasin
Email:
hasin.shaikh@gmail.com
Mobile:
+91-9924562942*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
Visit this group at
https://groups.google.com/group/materials-welding.
For more options, visit
https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
Visit this group at
https://groups.google.com/group/materials-welding.
For more options, visit
https://groups.google.com/d/optout.



 

--

*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...