Dear Experts,

We have an dissimilar WPS (P1 & P8) with combination process (GTAW - 8mm Max +SAMAW - 11.06 mm Max) upto 19.06 mm Thk 

The same WPS can be used for single process only (GTAW Upto 8 mm Max)

Please advise me with reference 