Yes can used, but it should be for P1 & P8 Material only.
Thanks & Regards,
Lakshman Kumar B,
+91 9440031459
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Amul Raj
Sent: Wednesday, December 13, 2017 8:41 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27176] combination process wps can be used only single process - reg
Dear Experts,
We have an dissimilar WPS (P1 & P8) with combination process (GTAW - 8mm Max +SAMAW - 11.06 mm Max) upto 19.06 mm Thk
The same WPS can be used for single process only (GTAW Upto 8 mm Max)
Please advise me with reference
Regards
Amul Raj T
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments