hi 


please be informed that minor grinding of welds is accepted if you check the 
welds by PT or MT.

BEST REGARDS 
H.SARPASI

On Sunday, December 10, 2017, 2:36:55 PM GMT+3:30, 'GOPU NAIR' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Amit

Minor grinding is permitted after hydraulic test.  

Gooal


On Sun, 10 Dec 2017 at 15:53, Amit Vishwakarma
<amitspvishwak@gmail.com> wrote:
Dear Experts,

Please give your advice on grinding of pressure vessel after the hydro test as during final visual inspection we couldn't find any surface damage on the shell but it has been discovered after surface preparation for painting. The pattern of surface defects on the shell can be been seen and it may be because of rolling of shell plate or job roller.
The vessel details as mentioned below & to meet the requirements of Aramco.

MOC SA240 Gr316L
Thickness 18mm
Size - Dia 3mtr x 20mt Length
Hydro Test Pressure 150PSI 
PWHT- NA

Kindly suggest it can be acceptable to remove defects by grinding maintaining min thickness of plate considering plate thickness tolerance.

Regards
Amit
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...