Wednesday, December 13, 2017

Re: [MW:27188] CRA-Weld overlay

If you use a Plate it will be 150mm x 150mm with 38mm wide of weld metal for necessary tests to be performed.

If you use a Pipe, length shall be 150mm and deposited weld shall be minimum of 38mm wide and it depends on the diameter to obtain the necessary test coupons.

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Wednesday, December 13, 2017, 4:52:46 PM GMT+4, venkkatesh krishnan <venkkateshkrishnan@gmail.com> wrote:


Dear Gents,

How much pipe length (for welding) is require for Corrosion Resistant Weld overlay Procedure qualification test per ASME Sec IX?

Per QW-453: required length is 150mm. Please tell me this entire length is to be welded.

Looking forward your reply

Regards,
Venkkatesh Gopalakrishnan.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...