Re: [MW:27145] NUMBER OF WELDERS ESTIMATION / CALCULATION REQUIRED FOR ONE API 650 STORAGE TANK CONSTRUCTION??...HOW TO CALCULATE? AND ESTIMATE THE WELDERS FOR TANK?

Mr. VIJAY can you please share your idea some more related to welders estimation 

Can i get more ways ? 

More hints regarding this topic 

On Sun, Oct 1, 2017 at 6:26 PM, Vijay Patre <vijay.patre09@gmail.com> wrote:
calculate welding inch dia for complete tank, as per required time for construction and accordingly calculate the welder requirement.

On Oct 1, 2017 2:09 PM, "API 650 TANK CONSTRUCTION" <gurunath.gm@gmail.com> wrote:
Hi

please any one guide me 

How to calculate the number of welders required for one tank construction? 

Any hints for welders estimation for one tank???????............any one give hints

Any Procedure for the estimation of no of welders required to be calculated for one API 650 storage tank construction work?

Please share your ideas and 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--


GURUNATH. M .G
CRUDE OIL TANKS ENGINEER

HYUNDAI ENG & CONST CO.LTD

SATAH AL RAZABOOT PLANT FACILITIES PROJECT

PACKAGE - 4 (SARB - P4)

P.O.Box 95016, 2nd Floor Al Fahim Group Building

Plot 8, M 4, Musaffah

Abu Dhabi. U.A.E

MOBILE       : +971502878681

E-MAIL ID    : - gurunath.sarbp4@hdec.co.kr

                          gurunath.gm@gmail.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...