Dear Experts
I need query on Aluminium welding
Material -6061-T6
Material Thickness-16mm
Filler wire- ER4046
Process-GMAW
Pre heat-70 centigrade
Interpass- 120 centigrade
Preclean by Acetone cleaner and SS wire brush
Gas-Ulta high purity Argon gas
During PQR qualifications we face failure in bend test. Crack open at 30degree itself. Is the above method required PWHT after welding. If so what is the method of PWHT and cycle.
Kindly clarify?
Thanks in advance
Regards
Sathish
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment