Range qualified will be 5--200. GMAW & FCAW treated identical for qualifications as per table QW -255.
On 28 Dec 2017 5:36 pm, "utreshwar" <utreshwarmiskin98@gmail.com> wrote:
hi--
can anyone know what is the range of qualification for 40mm thk plate (QW-403.8) for FCAW process. because QW-451 note-3 not shows FCAW process so confused. whether 2T or 5-200mm
On Sunday, 11 October 2009 10:53:27 UTC+5:30, Shashank Vagal wrote:
Hi Group Members,
Please see the following and advise.
Shashank Vagal
Query:
dear every one,
i have this problem i need to know the thickness range or pipes diameter range for the wps in which standard i think its in asme sec 9 but where ???
for exmple if i have wps for thickness 15 is it cover the 20 mm
waiting answer please
regards
My Reply:
A WPS is a guideline to ensure joint integrity as proven by PQR + applicable mech tests + NDT. It is intended for all job sizes once the welding technique used proves itself in these tests. The sizes etc come in to picture by qualifying welder on test coupons of a given size as per your job requirements. ASME IX stipulates weld metal deposit and not job size. Please ref to QW 450 - 461.
Now, send attachments up to 25MB with Yahoo! India Mail. Learn how.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.