Friday, December 8, 2017

[MW:27152] repair of damaged pipe ( wall thickness lost )

We have a feed water piping ( A 106  C ) thickness is 47 mm we remark a thickness lost of 3.5 to 4 mm( during supports modification ).

Our construction team propose to repair this damage by welding ( the same WPS used for production ) and after PWHT and NDE .

According your experience this solution it's acceptable or we should cut the damaged area and replace by new spool ?

regards

SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258