Dear PRADEEPKUMAR ,

Hydrotest file must contain :
- WPS , PQR and WPQR
- welding inspection reports.
- pipe installation reports
- pipe pigging reports
- NDE reports
- material certificates
- alignement sheet of the line with highest point , lowest point and the test points elevation
- water analysis
- corrosion inhibitor data sheet
- coating reports
- test equipments calibration certificates ( pressure gauge , dead weight tester ...)

Regards

SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258


Le jeudi 21 décembre 2017 à 05:25:42 UTC, Pradeep kumar hormis <pkhormis@gmail.com> a écrit :


Sirs

Could anyone can give me a sample copy of pipeline Hydrotest package index (contents).

Thanks & Regards

PRADEEPKUMAR HORMIS

Mob: +966-58 16 20 710



 
 


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...