RE: [MW:27204] Qualifications of welders

Yes

Final Conclusion in my opinion and based on the interpretation by Mr Jayakumar

Quote"

AS P Number and F number are essential variables for welder qualification and not A number. QW 423 provides exception for P-Number allowing both the ranges and F Number is same for SS & DSS.

 

AS per ASME Sec.iX it is permissible to use SS welder on DSS. Only thing in Dss welding Oxygen content in the purging gas has to be monitored and the welder educated on the same.

End Quote"

If a welder is qualified using coupon of P1 through P11 (Any material in between) he/she is qualified for welding P1 through P11 (Any material in between);

So he/she is already qualified for essential variable P No

Next is F number,

The F number of the electrodes used for both material is same.

So YES it is acceptable to use the same welder. As far as ASME BPV Section IX is concerned.

Regards,

Umar

 

From: 'ms viswanathan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: Wednesday, December 06, 2017 8:44 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27131] Qualifications of welders

 

Hai all,

 

What is your final conclusions.

 

Regards, M.S.Viswanathan

 

On Tuesday, December 5, 2017 9:45 PM, John Henning <jhenning@deltak.com> wrote:

 

Some care here needs to be applied and please remember to note that this applies only to welder performance qualification.

 

QW-423.1 refers to unassigned base metals.  In the case of unassigned base metals, generally the welder is only qualified for welding the unassigned base metal.

 

However,

 

QW-423.2 allows for base materials produced to other standards that meet the chemical and physical requirements of a P-Number material, to be used as if it were the P-number material for performance qualification.  This is an exception to the general rule stated in QW-423.1 for "unassigned" base metal. 

 

Enjoy

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hasin Shaikh
Sent: Monday, December 04, 2017 11:11 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27115] Qualifications of welders

 

Dear  Jhon Sir

 

As per QW 423.1 -unassigned material with similar chemical composition also included

in that case no need to go further new performance qualification if unassigned material have similar chemical composition with previous any qualification ,

 

This is my interpretation, is correct or not please advise.

 

With Regards

Hasin Shaikh

 

On Mon, Dec 4, 2017 at 9:22 PM, John Henning <jhenning@deltak.com> wrote:

No welder requalification is not required, provided all other requirements of QW-353 are met, and only Section IX qualification is required..

 

While Table QW-353 states QW-403.18 is an essential variable one has to look further.  QW-403.18 states:

 

 

So one has to look again further at QW-423, Alternate Base Materials for Welder Qualification:  There is no distinction made between P8 and P10H as far base material required is concerned.  In fact the welder could have qualified using P1  base materials for both P8 and P10H base metals.

 

However, customer requirements may restrict qualification. 

 

Clearly, applying the first instance in QW-423.1, performance qualification with P8 material

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PGoswami
Sent: Monday, December 04, 2017 9:28 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:27111] Qualifications of welders

 

 

A new qualification is required in this case. Qualification on other austenitic stainless steels(P No 8) does not permit the validity of qualification for duplex stainless steels (P No 10H). It's clearly stated under QW-353, please see the extract below.

 

F No for both ASS and DSS are the same, F5 for SMAW (SFA 5.5) and F6 for GTAW/GMAW(SFA 5.9).

 

Thanks.

 

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

 

 

QW-351 GENERAL

A welder shall be requalified whenever a change is

made in one or more of the essential variables listed for

each welding process

 

 

 

 

From: 'ms viswanathan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: December 4, 2017 7:23 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27109] Qualifications of welders

 

Yes, I agree .Thanks for your guidance.

 

Regards, M.S.Viswanathan

 

On Monday, December 4, 2017 1:46 PM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:

 

MSV

            pl see QW 416,423.

 A no is at all essential variable for welding performance qualification. Let us not misguide the people. 

 

Virus-free. www.avast.com


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

On Mon, Dec 4, 2017 at 3:51 PM, 'ms viswanathan' via Materials & Welding <materials-welding@googlegroups.com> wrote:

No, because DSS - P number is 10H and A.No-7 and .S.S-   P number is -8 and A.No 8 , essential variables.

 

Regards, M.S.Viswanathan

 

On Monday, December 4, 2017 12:42 PM, foued oudina <oudinafou21@gmail.com> wrote:

 

Dear Colleagues ;

 

 

Could you  please help me, we have welders qualified in SS they can weld DSS.

 

Thanks

 

 

 

 

 

OUDINA FOUAD | QC Welding OFF PLOT

 

Técnicas Reunidas Group

TouatGaz Project – EPCC Processing & Production Facilities

Field Engineering Group                   

Oued Zine, Adrar, Algeria

( Ext. 3912

 

 

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

 

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



 

--

*With Regards
Shaikh.Hasin
Email: hasin.shaikh@gmail.com
Mobile: +91-9924562942*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...