Saturday, December 9, 2017

Re: [MW:27156] Aluminum welding 6061-T6 mechanical test bend failure

Dear sir,

Please verify gas purity, I guess higher impurities added with carbon makes cracking.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


On Fri, Dec 8, 2017 at 11:03 PM, krishnan T <krishrev@gmail.com> wrote:
In my opinion No preheating, Aluminum oxide will form,breaking may be the reason . Try without preheating.

On 08-Dec-2017 4:09 PM, "Sathish Kumar" <sathishmech04@gmail.com> wrote:
Dear Experts
I need query on Aluminium welding
Material -6061-T6
Material Thickness-16mm
Filler wire- ER4046
Process-GMAW
Pre heat-70 centigrade
Interpass- 120 centigrade
Preclean by Acetone cleaner and SS wire brush
Gas-Ulta high purity Argon gas

During PQR qualifications we face failure in bend test. Crack open at 30degree itself. Is the above method required PWHT after welding. If so what is the method of PWHT and cycle.


Kindly clarify?


Thanks in advance
Regards
Sathish


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...