[MW:27222] Base Metal Qualified

Welding processes: GTAW/FCAW
Test Coupon thickness: 1.5"
GTAW weld size: 0.625; FCAW - 0.875"
What will be the base metal qualified range in WPS?
Maximum t For GTAW and FCAW?

Thank you in advance

--