Base metal: 3/16"-- 8"
Gtaw: 1.25"
Fcaw: 8"


On 25 Dec 2017 8:06 am, "Mikeyyc" <greenfield.mf@gmail.com> wrote:
Welding processes: GTAW/FCAW
Test Coupon thickness: 1.5"
GTAW weld size: 0.625; FCAW - 0.875"
What will be the base metal qualified range in WPS?
Maximum t For GTAW and FCAW?

Thank you in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...