Thursday, December 28, 2017

[MW:27229] Material Selection for Conveyor chain

Dear Experts.

Could anyone suggest the right material for a conveyor chain; following is the service condition:

Temperature: 450 deg C in one run and quenched by water in the return run,

Cargo: Sodium Silicate Flakes received in molten phase and conveyed in open air

Material currently being used: SS304 the life of the chain is 6months maximum.