[MW:27206] PWHT required or not for Saddle welded to pipes

Dear Expert 
                    Kindly help me out to decide whether we have to perform PWHT or not for Pipe to Saddle support fillet welding .Design  Code ASME B 31.1 .The details given below and its a long distance pipe rack job

The saddle material is ASTM A387 GR 11.
The welding type is fillet welding.
HP pipe detail - DN-350,THK-28 mm and Material  ASTM A 335 P11.

--
tHanks & rEgards
Chandra Bhanu Mohapatra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...