Re: [MW:26494] RE: WELD DISTANCE AS PER ASME [**EXTERNAL**]

Is that code requirement or nice to have?
HAZ is normally no more than 2-3 mm
If it is code please give paragraph number
 
Kind regards


Van: "pavan kumar reddy Juturu" <pavan2k20@gmail.com>
Aan: materials-welding@googlegroups.com
Verzonden: Zondag 30 april 2017 15:58:31
Onderwerp: Re: [MW:26493] RE: WELD DISTANCE AS PER ASME [**EXTERNAL**]

Dear Sir,

The distance between two weld joints should be 4 times the pipe wall thickness or one time the diameter of pipe but never closer than 1.5 inch. This is supposedly to prevent the overlap of HAZ of two joints.

Thanks and regards,
Pavankumar Reddy.

On Apr 23, 2017 4:19 PM, "Faizal, Majeed [c]" <FAIZAM@saudichevron.com> wrote:

Dear Amit,

 

I mean , what is the minimum distance between the nearest two socket weld joints.

 

faizal

 

 

From: Amit Vishwakarma [mailto:amitspvishwak@gmail.com]
Sent: Sunday, April 23, 2017 10:23 AM
To: Materials & Welding
Cc: Faizal, Majeed [c]
Subject: Re: WELD DISTANCE AS PER ASME [**EXTERNAL**]

 

*** WARNING: This email originated outside of the CPChem network. Use caution opening attachments, clicking web links, or replying. ***
-

Please find the snapshot of the code for your refrence. 

 

Regards

Amit Vishwakarma



On Sunday, April 23, 2017 at 11:31:07 AM UTC+5:30, Faizal, Majeed [c] wrote:

Can anyone please confirm the Minimum distance between Socket weld joint as per ASME B31.3 where its specified.

 

Regards,

 

Faizal

 

 

 

 

 


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2609A8F1CC683C46AAF25170C11C6B6D0A5C2E7B%40cpamsaaj-msx05.am.cpchem.net.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO4WkW%3DFVK2WJxt%2B9qkRkK8FJLaabdAhq__w9AfZ7DU9swBJPw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...