[MW:26518] Re: Selection of consumable for SA537 CL2 bullets

Hi,now we have a LPG sphere tank,material is SA537 CL2 thickness is 80mm,need PWHT ,Could you give me some suggest for welding electrode? thank you!
Regards' 
sun qiang

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...