Hi!
Basicaly before forming of DE you require to consider the reduction in wall thk in knuckle portion and accordigly you req to select higher thk. Plate for DE As this forming is carried by point pressing and followed by leveling or say dressing the surface by pressing to  level dents (to maintain min req wall thk )Dents are not acceptable and not to be repaired by welding for thk correction
Therefore one has to be careful during DE forming with due consideration to Die its surface n shape used and pressure applied
Regards
Hegde P.B


On Mon, 24 Apr 2017 at 17:14, anthony chundal
<anthony.chundal@gmail.com> wrote:
you can repair the same, provided you have a repair procedure,& a suitable Welding procedure. what is the minimum thickness required after forming,whether you are achieving the same before repair.

On Sun, Apr 23, 2017 at 5:44 PM, claire roberston <jamisburns@hotmail.co.uk> wrote:
A dent in material formation is not a welding defect. Can you include a photo. A weld repair is exactly that! A repair to the welded area. Otherwise it is a fabrication repair. Please clarify

--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ cc4538ad-966e-4e19-9b86- 5cafe3318697%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-ruFFWNikVwjAn0FwHVrD3WQyKJ8Qs1rSCr1mEt%2BLbig%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/603488647.7912321.1493037137246%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...