Re: [MW:26459] Preheat decrease >50deg.C

Just to add to Mr Mahadevans reply 
You req to preheat Even the thk of the job is very less(provided you use the same wps n spporting pqr) thete is no restriction on higher side preheat temp.
Regards
Hegde



On Sat, 22 Apr 2017 at 11:37, Kannayeram Gnanapandithan
<kgpandithan@gmail.com> wrote:
In PQR, if ur preheat temp is 100,℃, in wps u can mention minimum 45℃, ( 100-55=45,) if it is mentioned less 45, requalification required

On 21-Apr-2017 5:44 PM, "Vadivel Mahadevan" <vadivelmahadev@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (vadivelmahadev@gmail.com) Add cleanup rule | More info

Dear Experts,
I have a doubt.
In ASME sec. IX,in many Welding process it is mentioned as "Preheat decrease >55 deg. C"
can you let know what it means exactly..  How to intrepret this variable..
Thanks in advance
Vadivel M

--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
To post to this group, send email to materials-welding@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ cf10576a-f335-4b14-923d- 75e98c1e3165%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOM%2BgH%3DVPSunTQoqMp7SiLsk_X_xpsVo4D3eZvuZJB7-Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1319683990.6513531.1492846448591%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...