Re: [MW:26452] Welders Performance Monitoring

Dear ,

Please refer SEC IX for welder qualification(performance).
For welder qualification you have to maintain weld running sheet including heat input, current, voltage etc.
And NDT part may depend on client requirement.
RT is most common NDT method for welder qualification.

regards,
Rajendra Jadhav

On Thu, Apr 20, 2017 at 1:45 PM, ZAIDI Djahid <djahid.zaidi@gmail.com> wrote:
Dear Gents,

May I get a clarification about the welders performance Monitoring, is it 
by :Defect Inchs/Total inchs Welded
or by :RT Film Rejected/Total RT Film Taken
or by :Defect Inchs/Total Inchs Examinated with RT

For Information the NDT carried out by other subcontractor.

Is there any of that in standards?

Thanks in advance.

D. Zaidi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9dad54ce-1b97-41d1-b203-6312d759df97%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKtLVJzx_PgQbk2yGt%3D9JhMcWyrfs%3DP%3DpU9OdBhKC8PEbRjHNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...