Re: [MW:26432] Regarding Post Heating or Post Baking

Muni, it is not like that only p91 required. Other Steel materials also required Based on CE, Hardness, thickness etc. Pl ref ISO1011-2 for further details information

On 16-Apr-2017 9:11 PM, "C.Muni" <cmkfc07@gmail.com> wrote:
Post heating is  required for P91 material to avoid cracks.Other materials not required


On 11 Apr 2017 10:08 a.m., "Mohit Aggarwal" <aggarwalmohit05@gmail.com> wrote:
Dear Experts,

Kindly share the standard or code in which there is mention about post Heating of Alloy Steep materials like 
SA 335 P5 and SA 335 P9 etc.

Regards,
Mohit Aggarwal
9821958461

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPNOQS0jNPgxPwQgmMY1bn4WLnG2x00WsFVN%3DPuFC9U37Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMJSSYmMZQejxAdn-MbgZVomgV4rzbGFbvLVASiAv3__SSr-5Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM6J6wefV20p7PcfaUzTStVGnEsBQ1%3DhMeL46XY-Heugg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...