Can you please attach the results.For this welding preheating is handwarm. Interpass temperature is 200 deg C desirable.To pass in impact test,Some control in chemical composition n heat treatment required


On 16 Apr 2017 3:54 p.m., "A707 L5 CL#3" <prakashk210@gmail.com> wrote:
Hi All,
  • A707 L5 CL#3 15.8 mm Flange internal 6 mm overlay cladded with A625 inconell material required to join with API 5L X60 material.
  • Need to qualify a WPS by clad welding method using filler ER NiCrMo3 (GTAW) and E NiCrMo3 (SMAW)
  • A707 L5 CL#3 - CEV is 0.500
  • Toughness test requirement is supplementary essential. 
I need experts guidance for preparation of welding parameter, preheat and inter-pass temperature. Last two test failed on impact, hardness and Chemical tests.

Regards.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b7935f26-42da-4977-8838-8a52614e31ab%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMJSSYkgs-bNRkiUhsNN_ZA-K3GAMtKi0103eKn6FAsDBNj8Fw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...