Friday, April 14, 2017

Re: [MW:26412] PAUT (Phased Array Ultrasonic Testing)

Hi Firend
P/Array is reliable method can be used in liu of RT and very fast and no hazard
However you should have instrument and qualified person to carry and interprete the process

There are NDE/NDT vendors who take up the NDE by  P/Array  However you require to qualify the mock up prior to NDE test  depends upon thk,Metallurgy etc
Regards
Hegde


On Friday, 14 April 2017 11:04 AM, 'Ganesan' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Experts,

Can you please guide me regarding PAUT (Phased Array Ultrasonic Testing) instead of RT. Our contractor has recommended PAUT due to RT process is slow and it will be affected the project schedule. So, they are pressuring us to do PAUT instead of RT.  

Is it good NDT technique & which standard shall i follow for the acceptance criteria. 

Please share the testing method and acceptance criteria, if anyone have.

I'm waiting for your valuable advise in this regard.     
 
Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1547052087.1269331.1492067703665%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...