Friday, April 14, 2017

Re: [MW:26408] VACUUM TEST FOR SOTRAGE TANKS ROOF AS PER API 650

Dear,

To best of my knowledge - YES the air test of vented roof too is required. Let us both wait for some expert responses.

Good day.

Best Regards,

Vinod Bhatt

On Thu, Apr 13, 2017 at 10:42 AM, Pinto Antony <pintoantony81@gmail.com> wrote:
Dear Experts,

we are fabricating a dome roof oil tank with atmospheric venting this vent connected to the flame arrester, in this case, roof air test is required or not???

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8f9fe7d7-0fdd-447c-81d3-434e99b666e6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADC9dcncVf83gqL76nOYOBh4G7DaOt02jYHTOMJyz4g8%2BXNpXQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...