Re: [MW:26403] Re: Requirement of Solution Annealing for SS DIshed head after forming

check Table UHA-44.

Factors to consider are:
Alloy Grade
Design Temperature (lower and higher temperature range)
Strain after forming

The combination of the above factors is indicating if HT and at which temperature needs to be performed

2017-04-12 3:55 GMT+03:00 VIPUL <vipulagarwal19@gmail.com>:
Hi,

Please let me know What is the finishing forming temperature as per UHA-44.

Thanks,

Vipul

On Tuesday, 13 September 2011 15:48:03 UTC+5:30, asad azmi wrote:
Dear All,
 
Greetings.
 
SS Vessel is being fabricated as per construction code - ASME SEC VIII DIV 1
 
SERVICE : SOUR Service
 
Material of Construction  for Dished Head - SA 240 316L, 20 mm Thickness.
 
I  believe stresses will be  induced in the material  during forming and as a result , Sulfide Stress Cracking (SSC) failure may occur during operation.
 
Whether Solution Annealing of SS Dished Head is required after forming?
 
Please give reference of any International Standard.
 
Thanks & Regards
 
Asad Azmi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aaab94b5-9f51-44cf-98e3-2624725d6e2f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40ATLEGwaxjasJ4Mn9UMLSsU5dZ-XfH5QcrqVd%3D__4kq4A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...