Wednesday, April 19, 2017

[MW:26448] Fwd: Joint configuration in P91-reg



Dear experts,
                                        This is to inform u that we are manufacturer of Boiler components in India. In which one item called Flow nozzle made of P91 and SS316L as shown sketch attached.

your valuable comments are required on the following

1. Is this joint details acceptable for construction.

2.we had made 2 procedures.

   A). P91 was buttered with ER NiCr3 and PWHT
         After PWHT, these Buttered piece was joined with SS316 with Filler wire ERNiCr3.

     B) P91 and SS316 was directly welded with ERNiCr3 for Root and Hot pass
         Then balance welding was done by E9018-B9 and PWHT.

 In this we have faced with problem in procedure A) (Lack of fusion) and failed in service

your inputs are highly appreciated and thanks for ur cooperation.


THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM-n4dAgwBZJ%3DkC_hweOj0KgJZR_tHa-eg-xL3%3DAiFCPA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...