 Dear Sir,

 

 

We would like to ask some clarification

 

A.   Brief Summary

 

1.    The Welded Thermo-well to be welded as per Drawing below:

 

a.    Design Pressure : 10.4 barg  @ Plus (+) 75 degree C / Minus (-) 176 degree C

 

b.    Material : Weldolet : SS 316 and Thermowell : SS 316

 

2.    Item 5 Weldolet is welded to the Pipe

 

 

B.   Questions

 

a.    Is this weld considered full penetration weld (butt weld)?

 

b.    What is the Stress Concentration Factor (SCF)  for this weld?

 

c.    We have done Weld Strength Calculation Check, based on the calculation, Weld Leg Required is 0.804 mm (please refer to Attachment for calculation), this means the weld shown in the below Drawing is adequate. Please review and comment.

 

d.    If Argon Gas is not available for backing gas, can 100% Nitrogen be used? What are the precautions to be used?

 

e.    If backing gas is not possible, what other welding method is possible?

 

 

 

 

 

 

Thermo-well Drawings

 

 

 

 

 

 

 

 

 

 

 

 

Regards

 

Siva

 

Senior Mechanical Engineer

 

 



Virus-free. www.avg.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAH1%3DC0uAhEsbck8MGjM%2BmEA8CFVfQeMjpyPuf41XnFiFYibpg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...