[MW:26400] Filler wire for Copper materail

Dear All,
We have a Floating Head Cover assembly in exchanger which is having a material composition as follows:
Copper  : 68.5%.
Al         : 4.0%
Si         : 13.5%
Mn       : 7.6%
Fe        : 2.1%
Ni         : 1.4%
Zn        : 1.8%

Presently cracks are observed from weld and parent metal. Kindly advise suitable filler wire for carrying out repair work. We have tried to carry out welding with ERNi1 and ERNiCu7, but both time we are not successful. Presently we are thinking that may be ERCuMnNiAl can be used. Kindly provide your valuable suggestions. 

Requesting to also provide necessary preheat and interpass temperature parameters with comments.

Regards,
Devang Majithia

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFfyh2hWFK27hMxYCbzyTL9pKcbrdqWLaewg7VW%2BcK52PstBOw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...