HI,
 
Please refer AWS D1.1 and ABS Modu Part 2 , IACS 46/47: Only little info available in codes/stds in above said topic. Thanks
 


 
On Sun, Mar 17, 2013 at 2:29 AM, Anil Hegde <nott...@gmail.com> wrote:
Dear Expert ,

We have a 36 inch pipe which is welded type ,On it We have 12 inch connection which is coming on the ( long seam ) of the pipe .

Is There any code which says we can or cannot do welding on long seam of the pipe .

Requesting you for your positive feedback .

Regards
Anil Hegde 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Thanks & regards,

K.Babu
Singapore



***************************************************************************

PCMC Notice: "This email and its contents are confidential. If you are not the intended recipient, you are requested not to disclose or use the information contained in it. If you receive this e-mail in error, please notify us immediately by return email and delete the email and any attachments from your device. Statements and opinions expressed in this e-mail are those of the sender and do not necessarily reflect those of PCMC. PCMC and its employees accept no liability for any damage caused by any virus/error transmitted by this email

**************************************************************************************

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c12a23a8-6661-4069-9941-23c6cd871b01%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...