Re: [MW:26316] Combination of WPS and PQR

Dear Prasad

The properties will not affect if the correct consumables used, ensure that the essential variables are met for each welding process.

Regards
Govindan Perumal

On Mar 30, 2017 06:19, "Prasad Rode" <purode333@gmail.com> wrote:
Dear sir,

Thank for reply.
I ave referred the ASME sec is, clause QW200.4 a and b both. It is talking about base metal thickness and metal deposition thickness only.

My query is that, combination of these processes, doesn't affect the base metal properties?
i.e. all other essential variables of both processes does not required to be a compared. (means not required to be same).

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b2ae6081-4935-4a6c-a31d-e277846798cb%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9f7EAansphosFqE3cnEG7qKmwVc2i6-TW5LNY1xPok5Ow%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...