Re: [MW:26306] Combination or WPS and PQR

we can with in the limitation of all othervariables

On Sun, Mar 26, 2017 at 7:52 PM, Prasad Rode <purode333@gmail.com> wrote:
Dear sir,

I have two WPS and PQR separately.
1) SMAW up to 32mm
2) GMAW up to 32mm

But while using combination if these two process, is it necessary for me prepare separate PQR or by combining these two available PQR we can make third WPS.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37b8af07-fc52-4070-adb8-6e5c925c8712%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards
M.Sathyanarayanan

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzo-ks0QPVTi5fmSiqfiXo4EPWAG_CSGBBKLJZp%3DZeD%3D3ROSw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...