Wednesday, March 29, 2017

Re: [MW:26302] Circumferential pipe weld joint resting structural beam in process piping

Dear Sir,

  Perform RT and flush grind of the weld joint portion resting on beam and perform NDE accordingly and seek advice from engineering side

Regards

Raju Kandula

On Tue, Mar 28, 2017 at 11:19 PM, 'GENE MATSKO' via Materials & Welding <materials-welding@googlegroups.com> wrote:
1st. Check your job specifications for guidance for this unique situation.
2nd. Check your code of construction i.e. B31.3 B31.1 for same thing.
 In my opinion the weld joint should not be bearing on a structural member because you are unable to perform any full circumfrential
.NDE on the weld.
Also, over time the movement of the pipe in operation will wear away the weld.
Hope this helps.Remember: Measure two or more times and cut once to achieve minimal rework. 'Less is More'
 Sincerely,
Gene Matsko,小金




From: 'Biplab Pal' via Materials & Welding <materials-welding@googlegroups.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Tuesday, March 28, 2017 10:22 AM
Subject: [MW:26299] Circumferential pipe weld joint resting on structural beam in process piping

Dear experts,

We need your kind support based on your experience and any code/std references.

The situation is that some of our process piping in refinery division THE CIRCUMFERENTIAL JOINT has come such position that the joint rests on the structural beam.
Is it allowed?

Some inspector have a concern that there is a developed stress while operation and the joint may fail.

Please share your experience and reference.

Thank you very much 

With best regards
Biplab Pal
--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg22xWSiTOEonpZtZCDqBZ9vvh9OGZ_bKvHJ9CrS1L-qSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1486817357.7155956.1490732349381%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B8-Vvc%3DxnpWJLo7XeCKn0mXEfpyuMHCe%3DgA84JMZ0qT%3DA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...