Re: [MW:26296] Combination or WPS and PQR

Dear Prasad,
You can prepare the WPS with the combination of two PQRs in accordance with the clause QW200.4 (b)- ASME Section IX: 2015 Edition.

No need to prepare the PQRs, again, for more information please refer above clause in ASME Section IX.

Regards
Govindan Perumal

On Mar 27, 2017 15:31, "Prasad Rode" <purode333@gmail.com> wrote:
Dear sir,

I have two WPS and PQR separately.
1) SMAW up to 32mm
2) GMAW up to 32mm

But while using combination if these two process, is it necessary for me prepare separate PQR or by combining these two available PQR we can make third WPS.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37b8af07-fc52-4070-adb8-6e5c925c8712%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9f72i0_sLUDLU8UbbrcDT02YBzZ%3DKsUGMG%3Dd7W%2B0o9D5g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...